Home > News
Reason:Material water content is relatively large
Solution:
①Lengthen the time period of carbonization
②Control the moisture of the material below 25%
Reason:The size of carbonized raw materials is different
Solution:Try to place uniformly sized materials (below 10cm) in the carbonization furnace
Reason:
①The raw material is too wet
②The materials placed in the carbonization furnace are stacked too densely
Solution:
①Control the moisture content of raw materials below 25%
②Reduce the materials in the inner furnace
Reason:The interfaces are not tightly sealed
Solution:Strengthen the sealing of each interface